article · The European Physical Journal Plus
Abstract CaAl 2 O 4 :0.1% La nanoparticles doped with different concentrations of Mg were prepared using the sol–gel method and annealed at 400 °C, 500 °C, and 800 °C, respectively. The prepared nanophosphors show a highly crystalline orthorhombic structure with a crystallite size of about 81.2 nm. The optimum concentration of Mg dopants is about 0.7 mol%. The thermoluminescence (TL) glow curve of 11 Gy of beta-ray irradiated CaAl 2 O 4 :0.1% La:0.7% Mg measured at heating rates of 5 K/s has 16 overlapping glow peaks. The TL kinetic parameters for the prepared nanoparticles were evaluated using two different methods and they exhibited good agreement. Moreover, the linearity dose response of dosimetric peaks follows a good linearity up to 220 Gy in nanophosphor. The minimum detectable dose of the prepared nanophosphor was 125.7 mGy. The results of the prepared nanophosphors suggest good candidates for dosimetric applications. Graphical abstract
This page summarises published work. The authoritative version sits with the publisher.
DOI: 10.1140/epjp/s13360-024-05638-6
Is something wrong with this record? Report it or request removal.
Discussion
Have you built on this work, tried to replicate it, or seen it applied in practice? Share what you know. Verified researchers and MARATTO™ domain experts can open a discussion, and any member can reply. Contributions are reviewed before they appear.
No discussion yet. Open the first thread.
New to MARATTO™? Create a free account.