Improvement of Microstructural and Mechanical Characteristics of Friction Stir Welded AA6061 Aluminium Alloy Joint

20203 citationsOpen accessKafr el-Sheikh University

Abstract

Abstract To improve mechanical characteristics of friction stir welded joint made of AA6061-T6, AA2024 was used as a filler material due to its high strength and compatibility with AA6061 aluminium alloy. Different filler strip thickness (1, 1.5, and 2 mm) were investigated. Homogenous plastic deformation of the mixture with soft and refined grains was observed in the stir zone due to dynamic recrystallization of the grains. Friction stir welded joints with filler strip showed high hardness and tensile strength compared with filler-free joints. Welded joint with 1 mm filler strip has the highest tensile strength among other joints due to the dynamic recrystallization of the refined grains as a result of heat concentration. In addition, using greater thickness of filler strips makes the joining process more difficult, causes joint defects and reduces the tensile strength of welded joints.

Research topics

  • Advanced Welding Techniques Analysis
  • Aluminum Alloys Composites Properties
  • Aluminum Alloy Microstructure Properties

Read the original research

This page summarises published work. The authoritative version sits with the publisher.

DOI: 10.1088/1757-899x/751/1/012088

Is something wrong with this record? Report it or request removal.

Discussion

Discuss this research

Have you built on this work, tried to replicate it, or seen it applied in practice? Share what you know. Verified researchers and MARATTO™ domain experts can open a discussion, and any member can reply. Contributions are reviewed before they appear.

No discussion yet. Open the first thread.