article · Physicochemical Problems of Mineral Processing
In southwest China, the Panzhihua area annually produces about 80 million tons of tailings with a TiO<sub>2</sub> grade of around 5.0%, which causes serious waste of titanium resources as well as environmental and safety issues. The ilmenite contained in these tailings is ultra-fine in size, so it is difficult to recover under the regular operating conditions of pulsating high gradient magnetic separation (PHGMS). In this study, an SLon-100 PHGMS separator was applied to concentrate an ultra-fine titanium tailing under a wide range of operating conditions. The experimental results indicated that a combination of high pulsating frequency, large pulsating stroke, and low feed velocity was favorable for the highly efficient recovery of ultra-fine ilmenite from the tailings. The TiO<sub>2</sub> grade in the optimal concentrate was enhanced from 4.33% to 13.64%, at a recovery of 66.55% and an enrichment ratio of 3.15 through a one-stage PHGMS process. The size analysis of the optimal concentrate showed that the TiO<sub>2</sub> recovery in -25+18 µm and -18+10 µm fractions exceeded 70%. To further understand this PHGMS performance, the optimal ultra-fine ilmenite and larger-size ilmenite concentration conditions were compared. This study provides a valuable reference in the PHGMS operation for recovering ultra-fine weakly magnetic minerals, including ilmenite.
This page summarises published work. The authoritative version sits with the publisher.
DOI: 10.37190/ppmp/189617
Is something wrong with this record? Report it or request removal.
Discussion
Have you built on this work, tried to replicate it, or seen it applied in practice? Share what you know. Verified researchers and MARATTO™ domain experts can open a discussion, and any member can reply. Contributions are reviewed before they appear.
No discussion yet. Open the first thread.
New to MARATTO™? Create a free account.