Immediate dentin sealing increased the required debonding forces of occlusal veneers made of different materials and their bond strength without significant effect on their fracture resistance, however this improvement was found to be material dependant. All the used materials can withstand lateral and occlusal forces higher than the values recommended for restoring posterior teeth.